The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Geon® ALTC and ASTM D638 (formulation): 100phr Geon® 129, 57phr DINP, 3phr ESO, and 2phr Therm-Chek SP 120 LOHF Geon® STP 390(formulation): 100phr Geon® 129, and 60phr DOPInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Density 0.320 - 0.400 g/cc
0.0116 - 0.0145 lb/in³
ASTM D1505
Fineness 5.0
5.0
North Fineness; Geon® 390
Brookfield Viscosity 3.65 cP
3.65 cP
Initial, V12, Geon® 1010
5.43 cP
5.43 cP
One Day, V12, Geon® 1010
9.6 cP
9.6 cP
Initial, V20, Geon® 1253
12.2 cP
12.2 cP
One Day, V20
14.6 cP
14.6 cP
Initial, V2, Geon® 1253
19.2 cP
19.2 cP
One Day, V2
Viscosity Measurement 1.2
1.2
Inherent; ASTM D1243-60-A
Melt Flow 72 g/10 min

@Pressure 0.655 MPa
72 g/10 min

@Pressure 95.0 psi
Severs Efflux; Geon® 436
72 g/10 min

@Pressure 0.655 MPa
72 g/10 min

@Pressure 95.0 psi
Severs Efflux;
78 g/10 min

@Pressure 0.655 MPa
78 g/10 min

@Pressure 95.0 psi
Severs Efflux; Geon® 1010
Mechanical Properties Metric English Comments
Tensile Strength 22.4 MPa
3250 psi
Optimum; FF; ASTM D638
Elongation at Yield 0.00 %
0.00 %
FF; Optimum Tensile; ASTM D412
Optical Properties Metric English Comments
Gloss 61 %
61 %
60°, FF, ALTC-65
Transmission, Visible 68 %
68 %
FF, ATLC-66
Processing Properties Metric English Comments
Moisture Content 0.040 %
0.040 %
Karl Fisher-Geon® 683
Descriptive Properties Value Comments
Degree of Polymerization 1950
Correlation
Features Foamable
Low to No Fogging
Forms Powder
Gel Temperature 67 °C
FF, ALTC-29
Generic Material PVC Homopolymer
Generic Name Polyvinyl Chloride Homopolymer (PVC Homopolymer)
K-Value 0
No Standard; Correlation
82
ISO 174; Melt Flow Equivalent, DIN 53426
Methanol Extractables 3.6%
Geon® 894
Oil Immersion Fog Test 90
32°C; Film, 6 hr
Polymerization Process Dispersion
Processing Method Casting
Dip Coating
Rotational Molding
Vacuum Forming
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Automotive Interior Trim
Coating Applications
Fabrics
Users viewing this material also viewed the following: