Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 13000 cP @Temperature 23.9 °C |
13000 cP @Temperature 75.0 °F |
Mixed |
BCC Products BC 5200 Kwik-Set Adhesive BC5200 is a medium viscosity fast gelling two part Epoxy Adhesive System. With an easy to use 1 to 1 mix ratio, BC5200 is considered an excellent general purpose adhesive for in-shop use. BC5200 wil.. |
|||
Brookfield Viscosity | 13000 cP | 13000 cP | Thermosel using spindle #27 |
3M Scotch-Weld™ EZ250030 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th.. |
|||
Brookfield Viscosity | 13000 cP | 13000 cP | Thermosel using spindle #27 |
3M Scotch-Weld™ TE031 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Brookfield Viscosity | 13000 cP @Temperature 121 °C |
13000 cP @Temperature 250 °F |
|
3M Scotch-Weld™ 3755LM Low Melt Adhesive “Delayed-tack” applied in thin-glue-line ribbon for paper, corrugated, chipboard, displays, exhibits and Use with low melt applicator onlyInformation provided by 3M |