Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 14.6 cP | 14.6 cP | Initial, V2, Geon® 1253 |
PolyOne Geon™ 120 Series 129 Polyvinyl Chloride Homopolymer The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging.. |