Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 2.1 cP | 2.1 cP | Initial Viscosity @ 2 rpmGeon® ALTC 22 (with provided formulation); Internal Method |
PolyOne Geon™ FIT E 50 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® FIT E 50 is a low molecular weight homopolymer resin intended for use as a Formulation Improvement Tool (FIT) in plastisol formulations which enhance the plastisol usage (pot life) and reduce.. |
|||
Brookfield Viscosity | 2.1 cP | 2.1 cP | Initial Viscosity @ 2 rpmGeon® ALTC 22 (with provided formulation); Internal Method |
PolyOne Geon™ FIT E 52 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® FIT E 52 is a high molecular weight homopolymer resin intended for use as a Formulation Improvement Tool (FIT) in plastisol formulations which enhance the plastisol usage (pot life) and reduc.. |