Physical Properties Metric English Comments
Brookfield Viscosity 170000 - 200000 cP

@Temperature 25.0 °C
170000 - 200000 cP

@Temperature 77.0 °F
HBT, Spindle #SC4-14 @ 10rpm
Lord Adhesives Metech 3571 Silver Conductor Composition
This high performance silver conductor is designed for cost sensitive hybrid applications. It employs advanced powders technology with a mix bonded frit system to yield a highly dense fired film tha..