Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 2300 cP

@Temperature 25.0 °C
2300 cP

@Temperature 77.0 °F
0.2; MA 04-3-064
Dynasol Calprene® H6170 Hydrogenated Rubber SEBS
Calprene H 6170 is a 67/33 Ethylene-Butylene/Styrene thermoplastic copolymer, polymerized in solution and having a linear structure with excellent ozone resistance.This product is available in:CH 61..
Brookfield Viscosity 2300 cP
2300 cP
0.1; MA 04-3-064
Dynasol Calprene® H6174 Hydrogenated Rubber (SEBS)
Calprene H6174 is a 67/33 linear structure ethylene-butylene/styrene thermoplastic copolymer, polymerized in solution, with a high molecular weight and excellent ozone resistance. This product gives..
Brookfield Viscosity 2300 - 2700 cP
2300 - 2700 cP
Brookfield RVF sp 5, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A
Lubrizol Advanced Materials Pearlstick® 45-60/25 Polycaprolactone based TPU
Pearlstick 45-60/25 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a low thermoplasticity level. Solubili..