Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 2200 - 2700 cP @Temperature 20.0 °C |
2200 - 2700 cP @Temperature 68.0 °F |
Brookfield RVF sp. 4, 20 rpm solution at 15% in MEK; MQSA N° 40A |
Lubrizol Advanced Materials Pearlstick® 48-60/25 Linear Thermoplastic Polyurethane Elastomer Pearlstick 48-60/25 is an elastic, linear, aromatic polyurethane with a very high crystallization rate and a low-medium thermoplasticity level, available as pellets.Solubility: Pearlstick 48-60.. |
|||
Brookfield Viscosity | 2300 - 2700 cP | 2300 - 2700 cP | Brookfield RVF sp 5, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® 45-60/25 Polycaprolactone based TPU Pearlstick 45-60/25 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a low thermoplasticity level. Solubili.. |