Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | >= 3250 cP | >= 3250 cP | 0.3% in 1% HCl, LV3 rpm spindle n°2 after 24 h at 40°C; TI-2102-1 |
Solvay RHEOZAN Biopolymer Description: Biopolymer: very stable in acid media (such as sulfuric acid). Highly pseudoplastic.Identification: SUCCINOGLYCAN GUMCAS: 73667 – 50 – 2Available in: Asia Pacific, Europe, Lat.. |
|||
Brookfield Viscosity | 3250 cP @Temperature 23.9 °C |
3250 cP @Temperature 75.0 °F |
#2 spindle @ 20 rpm |
BCC Products METAL-KAST/SLO BC 8010-2 Urethane Casting BC8010-2 Metal-Kast/Slo, the result of extensive research and development is an aluminum filled, metal-like, medium setting urethane reproduction plastic. A slower version of the BC8010 Metal-Kast w.. |
|||
Brookfield Viscosity | 3250 cP | 3250 cP | melt viscosity |
Kuraray SEPTON® A1 Hot Melt Adhesive Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. Using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic block c.. |