Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 3500 - 8500 cP | 3500 - 8500 cP | DOP 60phr, 6RPM; ASTM D1824 |
LG Chemical PB900 PVC General Description: PB900, homopolymer made by micro-suspension seeded polymerization, is PVC resin with pseudo plastic flow property. PB900 can be used for wall paper made by knife coating/rotary .. |
|||
Brookfield Viscosity | 3500 - 4900 cP @Temperature 25.0 °C |
3500 - 4900 cP @Temperature 77.0 °F |
25% Toluene solution; BAM 922 |
Kraton® D1133 K (SBS) Linear Block Copolymer Description: Kraton D1133 K is a clear, linear triblock copolymer based on styrene and butadiene, with a polystyrene content of 36%. It is supplied from North America in the physical form identified.. |
|||
Brookfield Viscosity | 3500 cP | 3500 cP | #5, 20 RPM |
Dow BETAFOAM™ 89100 MDI-Based Urethane BETAFOAM™ 89100 is a component used to make low density, all water blown rigid polyurethane foam.Information provided by Dow |
|||
Brookfield Viscosity | 3500 cP @Temperature 23.9 °C |
3500 cP @Temperature 75.0 °F |
Mixed |
BCC Products BC 5003 Epoxy Laminating System BC 5003 is a medium viscosity, unfilled laminating system. It is a room temperature curing resin with a relatively short pot life. BC 5003 is also considered an excellent general purpose adhesive fo.. |