Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 10 - 40 cP | 10 - 40 cP | RVF #1 sp @ 20 rpm |
3M Fastbond™ 100 Lavender Foam Adhesive 3M™ Fastbond™ Foam Adhesive 100 is a one-part, water-dispersed, fast setting adhesive. The neoprene-based product bonds many porous substrates to porous or non-porous substrates with minimal dry t.. |
|||
Brookfield Viscosity | 10 - 40 cP | 10 - 40 cP | RVF #1 sp @ 20 rpm |