Material Notes:
3M™ Fastbond™ Foam Adhesive 100 is a one-part, water-dispersed, fast setting adhesive. The neoprene-based product bonds many porous substrates to porous or non-porous substrates with minimal dry time. Adheres to many types of flexible polyurethane foam, latex foam fabric, polyester fiberfill, wood, plywood, particleboard and many plastic and metal surfaces.Information provided by 3M
Physical Properties Metric English Comments
Density 1.08 - 1.13 g/cc
0.0390 - 0.0408 lb/in³
Solids Content 45 - 49 %
45 - 49 %
Brookfield Viscosity 10 - 40 cP
10 - 40 cP
RVF #1 sp @ 20 rpm
Mechanical Properties Metric English Comments
Peel Strength 0.158 kN/m
0.900 pli
Polypropylene
0.193 kN/m
1.10 pli
Aluminum
0.193 kN/m
1.10 pli
Galvanized Steel
0.193 kN/m
1.10 pli
Cold Rolled
0.263 kN/m
1.50 pli
Polyethylene
0.333 kN/m
1.90 pli
PVC
0.351 kN/m
2.00 pli
ABS
Descriptive Properties Value Comments
Appearance White (semi-transparent when dry)
Base Polychloroprene (neoprene)