Polymer Property : Brookfield Viscosity = 475 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 475 cP
475 cP
#2 Spindle, 30 rpm
Fibre Glast 77 Wax-Free General Purpose Polyester Molding Resin
Description:#77 Molding Resin is ideal for general purpose part fabrication and for building low cost molds. An internal thickening agent has been added to prevent drainage on vertical surfaces, yet..
Brookfield Viscosity 475 cP
475 cP
#2 Spindle, 30 rpm
Fibre Glast 83 Waxed Polyester Laminating Resin
Description: #83 Waxed Polyester Laminating Resin is a prepromoted, thixotropic general purpose resin. #83 contains styrene wax for low styrene emissions and to prevent air inhibition. #83 is a waxe..
Brookfield Viscosity 475 cP
475 cP
RVT Spindle #2, 20 rpm, 23°C, 15% TS in THF
Lubrizol ESTANE® 5701 Ester Based Thermoplastic Polyurethane
Features: Displays Low Temperature Flexibility and Abrasion Resistance.Uses: Audio Tape Binder and Screen Printing Inks, Inks and Lacquers, Cast Film for LaminationAvailable in Americas and AsiaInfo..