Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® 5701 Ester Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 5701 Ester Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Displays Low Temperature Flexibility and Abrasion Resistance.Uses: Audio Tape Binder and Screen Printing Inks, Inks and Lacquers, Cast Film for LaminationAvailable in Americas and AsiaInformation provided by Lubrizol
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Viscosity 2400 cP
2400 cP
RVT Spindle #2, 20 rpm, 23°C, 15% TS in Cyclohexanone
28000 cP

@Temperature 204 °C
28000 cP

@Temperature 399 °F
Melt; ASTM D1084-88
Brookfield Viscosity 475 cP
475 cP
RVT Spindle #2, 20 rpm, 23°C, 15% TS in THF
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ASTM D2240
Tensile Strength 49.0 MPa
7110 psi
ASTM D412/D638
Elongation at Break 460 %
460 %
ASTM D412/D638
100% Modulus 0.00520 GPa
0.754 ksi
300% Modulus 0.0131 GPa
1.90 ksi
Peel Strength 0.110 kN/m
0.628 pli
Adhesion to PET; TP-141
0.900 kN/m
5.14 pli
Aluminum Foil; ASTM D1867-72
5.00 kN/m
28.5 pli
Mylar Film; ASTM D1867-72
Thermal Properties Metric English Comments
Vicat Softening Point 70.0 °C
158 °F
ASTM D1525
Glass Transition Temp, Tg -23.0 °C
-9.40 °F
DSC
Ring & Ball Softening Point 161 °C
322 °F
ASTM E28-92
Descriptive Properties Value Comments
Gradient Bar Tack Temperature 121°C
Open Time <5 sec
ASTM D4497-94