Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 24000 - 80000 cP | 24000 - 80000 cP | RVT Spindle 3 @ 20 rpm |
Palm Labs Adhesives TURBO SEAL SERIES 85 WHITE STAINLESS STEEL THREAD SEALANT TURBO SEAL SERIES 95 is a medium strength high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The product cures rapidly in the absenc.. |
|||
Brookfield Viscosity | 40000 - 80000 cP | 40000 - 80000 cP | Accelerator, RFV #7 at 20 rpm |
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro.. |
|||
Brookfield Viscosity | 40000 - 80000 cP | 40000 - 80000 cP | Accelerator, RVF #7 spindle, 20 rpm |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |