Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 800000 - 1.20e+6 cP | 800000 - 1.20e+6 cP | Base, RVF #7 sp @ 2 rpm |
3M AC-645 B-2 Aerospace Sealant 3M Aerospace Sealant AC-645 B-2 is a low density, two-component, manganese dioxide cured, liquid polysulfide polymer system. It is suitable for use in fuel tanks, fuselage hole filling, cavity filli.. |