Material Notes:
3M Aerospace Sealant AC-645 B-2 is a low density, two-component, manganese dioxide cured, liquid polysulfide polymer system. It is suitable for use in fuel tanks, fuselage hole filling, cavity filling and fuel tank filleting applications. It has outstanding resistance to jet fuel, as well as resistance to chemicals, and petroleum products common to the aircraft industry. 3M AC-645 B-2 Sealant maintains its flexibility and bond strength on most meal substrates such as aluminum, titanium, steel, stainless steel, and many coatings under extremes of temperature, weathering and stress. The mixed compound is a thixotropic paste easily applied by extrusion, injection gun or spatula. It has excellent tooling properties.Information provided by 3M
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
cured 14 days @ 50% RH; STM 40-107
Volatiles 3.0 %
3.0 %
Brookfield Viscosity 70000 - 160000 cP
70000 - 160000 cP
Accelerator, RVF #7 sp @ 10 rpm
800000 - 1.20e+6 cP
800000 - 1.20e+6 cP
Base, RVF #7 sp @ 2 rpm
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
cured 14 days @ 50% RH; STM 40-107
Tensile Strength at Break 1.07 MPa
155 psi
Standard Cure; STM 40-107
0.827 MPa

@Temperature 60.0 °C,
Time 605000 sec
120 psi

@Temperature 140 °F,
Time 168 hour
STM 40-107
Elongation at Break 170 %
170 %
Standard Cure; STM 40-107
270 %

@Temperature 60.0 °C,
Time 605000 sec
270 %

@Temperature 140 °F,
Time 168 hour
STM 40-107
Peel Strength 3.16 kN/m
18.0 pli
Dry-Std, Alcad; STM 40-107
2.10 kN/m

@Temperature 60.0 °C,
Time 605000 sec
12.0 pli

@Temperature 140 °F,
Time 168 hour
JRF, Alcad; STM 40-107
2.10 kN/m

@Temperature 60.0 °C,
Time 6.05e+6 sec
12.0 pli

@Temperature 140 °F,
Time 1680 hour
JRF, Alcad; STM 40-107
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
STM 40-107, cured 14 days @ 50% RH
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
STM 40-107, cured 14 days @ 50% RH
Processing Properties Metric English Comments
Cure Time 1440 min
24.0 hour
Tack-Free Time
1440 min
24.0 hour
Shelf Life 9.00 Month

@Temperature <=26.7 °C
9.00 Month

@Temperature <=80.1 °F
Descriptive Properties Value Comments
Appearance Black
Black
Accelerator
Off White
Base