Polymer Property : Particle Mesh Size = 100 Mesh Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Mesh Size 60 - 100 Mesh
60 - 100 Mesh
Potters Industries Spheriglass® 1922 Solid Glass Spheres
Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage..
Particle Mesh Size 70 - 100 Mesh
70 - 100 Mesh
US Sieve
Potters Industries A-Series P-0080 Soda-Lime Silica Technical Quality Solid Glass Spheres
Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil..
Particle Mesh Size 60 - 100 Mesh
60 - 100 Mesh
0.0021
Gromax Melamine (Fine Grade)
China KInformation provided by Gromax Enterprises Corp.
Particle Mesh Size 60 - 100 Mesh
60 - 100 Mesh
0.1623
Gromax Standard GB9567-97
China NInformation provided by Gromax Enterprises Corp.
Particle Mesh Size 60 - 100 Mesh
60 - 100 Mesh
0.1973
Gromax Standard GB9567-97
China SInformation provided by Gromax Enterprises Corp.
Particle Mesh Size 80 - 100 Mesh
80 - 100 Mesh
Beijing Evergrow Resources ACFP-100 Activated Carbon Fiber Powder
Properties:High adsorption speed capacityGood efficiency towards pesticides and odorsPossible adaptation to condition of useHigh voluminal adsorption capacityRegenerableLow mineral contentApplicatio..