Gromax Standard GB9567-97

Category Polymer , Thermoset , Melamine
Manufacturer Gromax
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gromax Standard GB9567-97.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
China NInformation provided by Gromax Enterprises Corp.
Physical Properties Metric English Comments
Particle Mesh Size 10 - 32 Mesh
10 - 32 Mesh
0.0041
32 - 60 Mesh
32 - 60 Mesh
0.0215
60 - 100 Mesh
60 - 100 Mesh
0.1623
100 - 200 Mesh
100 - 200 Mesh
0.4865
200 - 325 Mesh
200 - 325 Mesh
0.2153
>= 325 Mesh
>= 325 Mesh
0.1103
pH 8.5
8.5
Maximum Moisture Content 0.040
0.040
Ash 0.0070 %
0.0070 %
Descriptive Properties Value Comments
Ammelide 0.0001
wt
0.0003
area
Ammeline 0.0006
wt
0.0019
area
Appearance White crystalline powder
Color 10
APHA
10
APHA
Gravity Ratio 0.65
Purity 0.999
HPLC, area
0.9993
HPLC, wt
Resolve 1
Time
clear
Test
Turbidity 2