Physical Properties Metric English Comments
Particle Mesh Size 45 - 60 Mesh
45 - 60 Mesh
US Sieve
Potters Industries A-Series P-0140 Soda-Lime Silica Technical Quality Solid Glass Spheres
Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil..
Particle Mesh Size 32 - 60 Mesh
32 - 60 Mesh
0
Gromax Melamine (Fine Grade)
China KInformation provided by Gromax Enterprises Corp.
Particle Mesh Size 32 - 60 Mesh
32 - 60 Mesh
0.0215
Gromax Standard GB9567-97
China NInformation provided by Gromax Enterprises Corp.
Particle Mesh Size 32 - 60 Mesh
32 - 60 Mesh
0.0473
Gromax Standard GB9567-97
China SInformation provided by Gromax Enterprises Corp.