Physical Properties Metric English Comments
Surface Tension 36.5 dynes/cm
36.5 dynes/cm
Dow Corning 705 DIFFUSION PUMP FLUID
A colorless, penta phenyltrisiloxane, single-component fluid designed for ultrahigh vacuums of 10-10 torr (untrapped) and 10-11 (trapped).Information provided by Dow Corning