Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Surface Tension = 38 dynes/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Surface Tension 36 - 38 dynes/cm
36 - 38 dynes/cm
1st surface; units: Dyne; Dyne Pens
SABIC Innovative Plastics Lexan® FR700 Polycarbonate Film, Flame Retardant
Lexan FR700 is a black, one side fine matt, one side velvet flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good d..
Surface Tension 36 - 38 dynes/cm
36 - 38 dynes/cm
2nd surface; units: Dyne; Dyne Pens
SABIC Innovative Plastics Lexan® FR700 Polycarbonate Film, Flame Retardant
Lexan FR700 is a black, one side fine matt, one side velvet flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good d..
Surface Tension 36 - 38 dynes/cm
36 - 38 dynes/cm
1st surface; units: Dyne; Dyne Pens
SABIC Innovative Plastics Lexan® FR735A Polycarbonate Film, Flame Retardant
Lexan FR735A is a black, one side velvet, one polish flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good dimensio..
Surface Tension 36 - 38 dynes/cm
36 - 38 dynes/cm
2nd surface; units: Dyne; Dyne Pens
SABIC Innovative Plastics Lexan® FR735A Polycarbonate Film, Flame Retardant
Lexan FR735A is a black, one side velvet, one polish flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good dimensio..
Surface Tension 36 - 38 dynes/cm
36 - 38 dynes/cm
untreated side; ASTM D2578
Honeywell Oxyshieldâ„¢ BOEB Biaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film
Description: Oxyshieldâ„¢ BOEB is a 0.60 mil (15 micron) biaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of relative humidity. T..
Surface Tension 28 - 38 dynes/cm
28 - 38 dynes/cm
Ring Type; LSY-QB-ID005
LG Chemical Lutex 105 NBR Latex
Description: Tensile strength, Elongation, Oil resistance, Abrasion resistance, Softness, WhitenessApplication: Nitrile Glove (Examination Glove, Clean Room Glove), Supported Glove (Industrial Glove..