Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 36 - 38 dynes/cm | 36 - 38 dynes/cm | 1st surface; units: Dyne; Dyne Pens |
SABIC Innovative Plastics Lexan® FR700 Polycarbonate Film, Flame Retardant Lexan FR700 is a black, one side fine matt, one side velvet flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good d.. |
|||
Surface Tension | 36 - 38 dynes/cm | 36 - 38 dynes/cm | 2nd surface; units: Dyne; Dyne Pens |
SABIC Innovative Plastics Lexan® FR700 Polycarbonate Film, Flame Retardant Lexan FR700 is a black, one side fine matt, one side velvet flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good d.. |
|||
Surface Tension | 36 - 38 dynes/cm | 36 - 38 dynes/cm | 1st surface; units: Dyne; Dyne Pens |
SABIC Innovative Plastics Lexan® FR735A Polycarbonate Film, Flame Retardant Lexan FR735A is a black, one side velvet, one polish flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good dimensio.. |
|||
Surface Tension | 36 - 38 dynes/cm | 36 - 38 dynes/cm | 2nd surface; units: Dyne; Dyne Pens |
SABIC Innovative Plastics Lexan® FR735A Polycarbonate Film, Flame Retardant Lexan FR735A is a black, one side velvet, one polish flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good dimensio.. |
|||
Surface Tension | 36 - 38 dynes/cm | 36 - 38 dynes/cm | untreated side; ASTM D2578 |
Honeywell Oxyshieldâ„¢ BOEB Biaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film Description: Oxyshieldâ„¢ BOEB is a 0.60 mil (15 micron) biaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of relative humidity. T.. |
|||
Surface Tension | 28 - 38 dynes/cm | 28 - 38 dynes/cm | Ring Type; LSY-QB-ID005 |
LG Chemical Lutex 105 NBR Latex Description: Tensile strength, Elongation, Oil resistance, Abrasion resistance, Softness, WhitenessApplication: Nitrile Glove (Examination Glove, Clean Room Glove), Supported Glove (Industrial Glove.. |