Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 33 - 43 dynes/cm | 33 - 43 dynes/cm | |
Dow Latex XZ 92199.00 Experimental Latex Description: XZ 92199.00 Experimental latex is an aqueous dispersion of a modified carboxylated styrene butadiene copolymer. It has been developed for use as an adhesive latex for secondary backed t.. |