Physical Properties Metric English Comments
Surface Tension 47 dynes/cm
47 dynes/cm
Harmonic Mean - Total
Eastman Eastman Embrace Copolyester for Shrink Film
Applications:Flexible packagingIV containersLabels to fit high contour containersShrink packagingWrap around designKey Attributes:Excellent clarityExcellent printabilityGood chemical resistanceGood ..
Surface Tension 47 dynes/cm
47 dynes/cm
Total; ASTM D5946
Eastman Tritan FX200 Copolyester
Eastman Tritan FX200 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w..