Polymer Property : High Load Melt Index = 70 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
High Load Melt Index 70 g/10 min

@Load 21.6 kg,
Temperature 190 °C
70 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Premix Thermoplastics PRE-ELEC® PE 1294
PRE-ELEC PE 1294 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129..
High Load Melt Index 70 g/10 min

@Load 21.6 kg,
Temperature 200 °C
70 g/10 min

@Load 47.6 lb,
Temperature 392 °F
ISO 1133
Premix Thermoplastics PRE-ELEC® PS 1328
PRE-ELEC PS 1328 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ..