Polymer Property : High Load Melt Index = 8.3 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
High Load Melt Index 8.3 g/10 min

@Load 21.6 kg,
Temperature 190 °C
8.3 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Chevron Phillips Marlex® HXM 50100-02 Extra high molecular weight hexene copolymer  (discontinued **)
Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesCharacteristics:..
High Load Melt Index 8.3 g/10 min

@Load 21.6 kg,
Temperature 190 °C
8.3 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Dow DGDB-2480 NT High Density Polyethylene Resin
DOW DGDA-2475 NT is produced using UNIPOL™ process technology. It is intended for use in pipe applications where long term hydrostatic strength and resistance to slow crack growth are desired. Su..