Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 8.3 g/10 min @Load 21.6 kg, Temperature 190 °C |
8.3 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips Marlex® HXM 50100-02 Extra high molecular weight hexene copolymer
(discontinued **) Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesCharacteristics:.. |
|||
High Load Melt Index | 8.3 g/10 min @Load 21.6 kg, Temperature 190 °C |
8.3 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Dow DGDB-2480 NT High Density Polyethylene Resin DOW DGDA-2475 NT is produced using UNIPOL™ process technology. It is intended for use in pipe applications where long term hydrostatic strength and resistance to slow crack growth are desired. Su.. |