Physical Properties Metric English Comments
Bead Size 0.400 - 0.800 mm
0.0157 - 0.0315 in
SABIC EPS 452 Expandable Polystyrene
Product Description: Standard expanded Polystyrene EPS 452 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
NOVA Chemicals Dytherm® 170R Expandable Polystyrene
This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
NOVA Chemicals Dytherm® 270R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
NOVA Chemicals Dytherm® 370R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Bead Size 0.400 - 0.800 mm
0.0157 - 0.0315 in
NOVA Chemicals Styrocell® B733A Expandable Polystyrene  (discontinued **)
This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used as expansion agent, typically used as pre-expanded beads in the ..
Bead Size 0.400 - 0.800 mm
0.0157 - 0.0315 in
Breda Laboratory Analytical Methods 90.30
NOVA Chemicals Styrocell® B733A Expandable Polystyrene  (discontinued **)
This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used as expansion agent, typically used as pre-expanded beads in the ..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
Ineos Nova Styrocell® M742C Expandable Polystyrene
A high strength regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell M742C is used ma..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
Ineos Nova T733B Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used after expansion for cellular bricks.Applications: This grade is..
Bead Size 0.400 - 0.900 mm
0.0157 - 0.0354 in
IRPC Polimaxx Pentfoam 361F Expandable Polystyrene
GENERAL: PENTFOAM "361F" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST MOLDING CYCLES IN V..
Bead Size 0.400 - 0.710 mm
0.0157 - 0.0280 in
IRPC Polimaxx Pentfoam 455E Expandable Polystyrene
GENERAL: PENTFOAM "455E" IS A SELF EXTINGUISHING (SE) GRADE EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST CYCLES IN VACUUM MOL..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
Jackon JACKOCELL® R411 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionThe unique design of polystyrene chains and additive chemistry in the Jackocell® R411 gives pre-expanded beads of high dimensional stability. The R411 represents the..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
BASF Styropor® F 415-N Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: For the manufacture of flame-retardant foamsApplications: Visible cover pa..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
BASF Styropor® F 495-N Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
BASF Styropor® P 426 Expandable Polystyrene
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Thin-walled molded parts.Information pr..
Bead Size 0.400 - 0.900 mm
0.0157 - 0.0354 in
IRPC Polimaxx Pentfoam 422F Expandable Polystyrene
GENERAL: PENTFOAM "422F" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST MOLDING CYCLES IN V..
Bead Size 0.400 - 0.900 mm
0.0157 - 0.0354 in
IRPC Polimaxx Pentfoam 522F Expandable Polystyrene
GENERAL: PENTFOAM "522F" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST MOLDING CYCLES IN V..
Bead Size 0.400 - 0.900 mm
0.0157 - 0.0354 in
IRPC Polimaxx Pentfoam 526W Expandable Polystyrene
GENERAL: PENTFOAM "526W" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT.APPLICATIONS: PENTFOAM "526W" IS PARTICULARLY WELL SUITED FOR THE MANUFA..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
Breda Laboratory Analytical Methods 90.30
NOVA Chemicals Styrocell® D733A Expandable Polystyrene  (discontinued **)
This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for contour molding.Applications: This grade is used for dry mol..
Bead Size 0.400 - 0.800 mm
0.0157 - 0.0315 in
SABIC EPS 450FF Expandable Polystyrene
Product Description: Fire retardant expanded Polystyrene EPS 450FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch proce..
Bead Size 0.400 - 0.700 mm
0.0157 - 0.0276 in
BASF Styropor® P 426 C Expandable Polystyrene
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Thin-walled molded parts with very shor..
Bead Size 0.400 - 0.900 mm
0.0157 - 0.0354 in
IRPC Polimaxx Pentfoam 328H Expandable Polystyrene
General: Pentfoam 328H is a high density grade expandable polystyrene containing pentane as blowing agent, this grade is developed to meet the demand for fast molding cycles in vacuum machineApplica..