Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 0.300 - 0.700 mm | 0.0118 - 0.0276 in | |
NOVA Chemicals Dytherm® 170F Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Bead Size | 0.300 - 0.700 mm | 0.0118 - 0.0276 in | Breda Laboratory Analytical Methods 90.30 |
NOVA Chemicals Dytherm® 170R Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Bead Size | 0.300 - 0.700 mm | 0.0118 - 0.0276 in | Breda Laboratory Analytical Methods 90.30 |
NOVA Chemicals Dytherm® 270R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Bead Size | 0.300 - 0.700 mm | 0.0118 - 0.0276 in | Breda Laboratory Analytical Methods 90.30 |
NOVA Chemicals Dytherm® 370R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Bead Size | 0.300 - 0.500 mm | 0.0118 - 0.0197 in | Breda Laboratory Analytical Methods 90.30 |
NOVA Chemicals Styrocell® D833A Expandable Polystyrene
(discontinued **) This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for dry molding of drinking cups and thin wall containers.Applic.. |
|||
Bead Size | 0.300 - 0.500 mm | 0.0118 - 0.0197 in | |
Iran Petrochemical (PCC) TPC - 522 FC Expandable Polystyrene TPC - 522 FCApplications: shape molding with wall thickness |
|||
Bead Size | 0.300 - 0.500 mm | 0.0118 - 0.0197 in | |
Iran Petrochemical (PCC) TPC - 526 WP Expandable Polystyrene TPC - 526 WPApplications: very thin-wall water proof shape molding products with wall thickness |
|||
Bead Size | <= 0.300 mm | <= 0.0118 in | |
Iran Petrochemical (PCC) TPC - 600 EX Expandable Polystyrene TPC - 600 EXSpecial type for extrusionInformation provided by Iran Petrochemical Commercial Co. |
|||
Bead Size | 0.300 - 0.700 mm | 0.0118 - 0.0276 in | |
BASF Styropor® P 570 Expandable Polystyrene Additive Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Only foamed particles, good foaming capacity.Applications: For the production of expanded particles as a filling material .. |