Physical Properties Metric English Comments
Bead Size 0.300 - 0.700 mm
0.0118 - 0.0276 in
NOVA Chemicals Dytherm® 170F Expandable Polystyrene
This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive..
Bead Size 0.300 - 0.700 mm
0.0118 - 0.0276 in
Breda Laboratory Analytical Methods 90.30
NOVA Chemicals Dytherm® 170R Expandable Polystyrene
This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive..
Bead Size 0.300 - 0.700 mm
0.0118 - 0.0276 in
Breda Laboratory Analytical Methods 90.30
NOVA Chemicals Dytherm® 270R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Bead Size 0.300 - 0.700 mm
0.0118 - 0.0276 in
Breda Laboratory Analytical Methods 90.30
NOVA Chemicals Dytherm® 370R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Bead Size 0.300 - 0.500 mm
0.0118 - 0.0197 in
Breda Laboratory Analytical Methods 90.30
NOVA Chemicals Styrocell® D833A Expandable Polystyrene  (discontinued **)
This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for dry molding of drinking cups and thin wall containers.Applic..
Bead Size 0.300 - 0.500 mm
0.0118 - 0.0197 in
Iran Petrochemical (PCC) TPC - 522 FC Expandable Polystyrene
TPC - 522 FCApplications: shape molding with wall thickness
Bead Size 0.300 - 0.500 mm
0.0118 - 0.0197 in
Iran Petrochemical (PCC) TPC - 526 WP Expandable Polystyrene
TPC - 526 WPApplications: very thin-wall water proof shape molding products with wall thickness
Bead Size <= 0.300 mm
<= 0.0118 in
Iran Petrochemical (PCC) TPC - 600 EX Expandable Polystyrene
TPC - 600 EXSpecial type for extrusionInformation provided by Iran Petrochemical Commercial Co.
Bead Size 0.300 - 0.700 mm
0.0118 - 0.0276 in
BASF Styropor® P 570 Expandable Polystyrene Additive
Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Only foamed particles, good foaming capacity.Applications: For the production of expanded particles as a filling material ..