Polymer Property : Bead Size = 0.0480 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bead Size 1.22 - 1.40 mm
0.0480 - 0.0551 in
BASF Styropor® KF 162M EPS
Description: Expandable polystyrene (EPS) with pentane as a blowing agent. For the production of expanded foam. Block having bulk densities of 12-30 kg/m3 and fire characteristics in conformity with..