Polymer Property : Bead Size = 1.40 mm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bead Size 0.900 - 1.40 mm
0.0354 - 0.0551 in
SABIC EPS 650FF Expandable Polystyrene
Product Description: Fire retardant expanded Polystyrene EPS 650FF is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch proce..
Bead Size 0.900 - 1.40 mm
0.0354 - 0.0551 in
SABIC EPS 652 Expandable Polystyrene
Product Description: Standard expanded Polystyrene EPS 652 is manufactured by the suspension polymerization of styrene monomer. The polymerization is generally carried out in a batch process. EPS..
Bead Size 1.00 - 1.40 mm
0.0394 - 0.0551 in
Ineos Nova Styrocell® M442C Expandable Polystyrene
A high strength, fast cycling regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell M4..
Bead Size 1.00 - 1.40 mm
0.0394 - 0.0551 in
Ineos Nova T443C Expandable Polystyrene
A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for low and standard density foam.Applications: This grade is us..
Bead Size 0.800 - 1.40 mm
0.0315 - 0.0551 in
BASF Neopor® 2300 Expandable Polystyrene
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider..
Bead Size 1.22 - 1.40 mm
0.0480 - 0.0551 in
BASF Styropor® KF 162M EPS
Description: Expandable polystyrene (EPS) with pentane as a blowing agent. For the production of expanded foam. Block having bulk densities of 12-30 kg/m3 and fire characteristics in conformity with..
Bead Size 0.700 - 1.40 mm
0.0276 - 0.0551 in
> 95% in this range per Berre Laboratory Analytical Methods 0492
Ineos Nova W441A Expandable Polystyrene
A regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for high density foam applications.Applications: This grade is sued mainly for..