Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 0.420 - 0.820 mm | 0.0165 - 0.0323 in | > 95% in this range per Berre Laboratory Analytical Methods 0492 |
Ineos Nova T733B Expandable Polystyrene A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used after expansion for cellular bricks.Applications: This grade is.. |