Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 1.00 - 2.00 mm | 0.0394 - 0.0787 in | |
BASF Styropor® F 215 N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing a uniformly distributed ?ame retardant (blowing agent: pentane)Remarks: For the manufacture of flame-retardant foams.Applications: Blocks, insula.. |
|||
Bead Size | 1.00 - 2.00 mm | 0.0394 - 0.0787 in | |
BASF Styropor® F 215 L-N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing a uniformly distributed came retardant (blowing agent: pentane)Remarks: For the manufacture of flame-retardant foams.Applications: Low-density bl.. |