Polymer Property : Viscosity Test = 0.90 cm³/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Test 0.90 cm³/g
0.90 cm³/g
Inherent, 0.5% solution in 98%H2SO4; ASTM D2857
Gharda Chemicals GATONE™ 5300PF Polyetheretherketone (PEEK)  (discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..