Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Test 205 cm³/g
205 cm³/g
Viscosity number
BASF Ultramid® A34 01 PA66 (Conditioned)
Ultramid A34 01 is an intermediate visosity, PA66 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or ..
Viscosity Test 205 cm³/g
205 cm³/g
Viscosity number
BASF Ultramid® A34 01 PA66 (Dry)
Ultramid A34 01 is an intermediate visosity, PA66 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or ..