Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 63.0 - 81.0 cm³/g | 63.0 - 81.0 cm³/g | Average value: 68.4 cm³/g Grade Count:5 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |