Overview of materials for Polysulfone (PSU)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polysulfone (PSU).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.13 - 1.72 g/cc
0.0408 - 0.0621 lb/in³
Average value: 1.37 g/cc Grade Count:195
Filler Content 2.00 - 40.0 %
2.00 - 40.0 %
Average value: 16.5 % Grade Count:40
Water Absorption 0.00300 - 1.70 %
0.00300 - 1.70 %
Average value: 0.348 % Grade Count:98
Moisture Absorption at Equilibrium 0.100 - 0.600 %
0.100 - 0.600 %
Average value: 0.236 % Grade Count:28
Water Absorption at Saturation 0.300 - 1.60 %
0.300 - 1.60 %
Average value: 0.996 % Grade Count:17
Additive Loading 10.0 - 30.0 %
10.0 - 30.0 %
Average value: 16.3 % Grade Count:4
Viscosity Test 63.0 - 81.0 cm³/g
63.0 - 81.0 cm³/g
Average value: 68.4 cm³/g Grade Count:5
Linear Mold Shrinkage 0.0000900 - 0.0130 cm/cm
0.0000900 - 0.0130 in/in
Average value: 0.00459 cm/cm Grade Count:164
Linear Mold Shrinkage, Transverse 0.00250 - 0.0135 cm/cm
0.00250 - 0.0135 in/in
Average value: 0.00644 cm/cm Grade Count:37
Melt Flow 3.00 - 90.0 g/10 min
3.00 - 90.0 g/10 min
Average value: 18.9 g/10 min Grade Count:40
Mechanical Properties Metric English Comments
Hardness, Rockwell M 68.0 - 92.0
68.0 - 92.0
Average value: 78.5 Grade Count:13
Hardness, Rockwell R 110 - 128
110 - 128
Average value: 122 Grade Count:32
Hardness, Shore D 80.0 - 86.0
80.0 - 86.0
Average value: 81.2 Grade Count:5
Ball Indentation Hardness 115 - 227 MPa
16700 - 32900 psi
Average value: 153 MPa Grade Count:11
Tensile Strength, Ultimate 6.00 - 185 MPa
870 - 26800 psi
Average value: 86.9 MPa Grade Count:161
50.0 - 125 MPa

@Temperature 0.000 - 160 °C
7250 - 18100 psi

@Temperature 32.0 - 320 °F
Average value: 67.6 MPa Grade Count:4
20.0 - 55.0 MPa

@Temperature 160 - 160 °C
2900 - 7980 psi

@Temperature 320 - 320 °F
Average value: 67.6 MPa Grade Count:2
20.0 - 55.0 MPa

@Strain 1.00 - 2.00 %
2900 - 7980 psi

@Strain 1.00 - 2.00 %
Average value: 67.6 MPa Grade Count:2
Tensile Strength, Yield 48.0 - 185 MPa
6960 - 26800 psi
Average value: 87.9 MPa Grade Count:54
40.0 - 68.0 MPa

@Temperature 60.0 - 140 °C
5800 - 9860 psi

@Temperature 140 - 284 °F
Average value: 55.3 MPa Grade Count:1
Elongation at Break 0.500 - 110 %
0.500 - 110 %
Average value: 16.5 % Grade Count:181
1.60 - 2.50 %

@Temperature 60.0 - 235 °C
1.60 - 2.50 %

@Temperature 140 - 455 °F
Average value: 27.9 % Grade Count:5
Elongation at Yield 0.200 - 10.0 %
0.200 - 10.0 %
Average value: 2.51 % Grade Count:39
2.80 - 4.50 %

@Temperature 60.0 - 150 °C
2.80 - 4.50 %

@Temperature 140 - 302 °F
Average value: 3.70 % Grade Count:1
Modulus of Elasticity 1.80 - 35.2 GPa
261 - 5100 ksi
Average value: 5.72 GPa Grade Count:175
1.90 - 9.00 GPa

@Temperature 50.0 - 200 °C
276 - 1310 ksi

@Temperature 122 - 392 °F
Average value: 7.30 GPa Grade Count:7
Flexural Yield Strength 71.0 - 255 MPa
10300 - 37000 psi
Average value: 130 MPa Grade Count:176
Flexural Modulus 0.103 - 19.3 GPa
14.9 - 2800 ksi
Average value: 5.43 GPa Grade Count:176
Compressive Yield Strength 13.0 - 176 MPa
1890 - 25500 psi
Average value: 88.4 MPa Grade Count:13
Compressive Modulus 1.73 - 2.59 GPa
251 - 375 ksi
Average value: 2.30 GPa Grade Count:3
Shear Modulus 0.0250 - 1.00 GPa

@Temperature 50.0 - 225 °C
3.63 - 145 ksi

@Temperature 122 - 437 °F
Average value: 0.688 GPa Grade Count:5
Shear Strength 62.1 - 68.9 MPa
9000 - 10000 psi
Average value: 63.4 MPa Grade Count:6
Secant Modulus 0.0250 - 0.950 GPa

@Temperature 50.0 - 200 °C
3.63 - 138 ksi

@Temperature 122 - 392 °F
Average value: 0.669 GPa Grade Count:1
Izod Impact, Notched 0.267 - 6.90 J/cm
0.500 - 12.9 ft-lb/in
Average value: 0.806 J/cm Grade Count:159
Izod Impact, Unnotched 2.40 J/cm - NB
4.50 ft-lb/in - NB
Average value: 6.74 J/cm Grade Count:91
Izod Impact, Notched (ISO) 4.00 - 10.0 kJ/m²
1.90 - 4.76 ft-lb/in²
Average value: 6.84 kJ/m² Grade Count:36
5.00 - 13.0 kJ/m²

@Temperature -30.0 - 120 °C
2.38 - 6.19 ft-lb/in²

@Temperature -22.0 - 248 °F
Average value: 7.44 kJ/m² Grade Count:6
Izod Impact, Unnotched (ISO) 23.0 kJ/m² - NB
10.9 ft-lb/in² - NB
Average value: 48.0 kJ/m² Grade Count:31
36.0 - 50.0 kJ/m²

@Temperature -25.0 - 120 °C
17.1 - 23.8 ft-lb/in²

@Temperature -13.0 - 248 °F
Average value: 41.3 kJ/m² Grade Count:1
Charpy Impact Unnotched 3.00 J/cm² - NB
14.3 ft-lb/in² - NB
Average value: 3.95 J/cm² Grade Count:19
4.00 J/cm² - NB

@Temperature -30.0 - -20.0 °C
19.0 ft-lb/in² - NB

@Temperature -22.0 - -4.00 °F
Average value: 4.13 J/cm² Grade Count:9
Charpy Impact, Notched 0.350 - 1.50 J/cm²
1.67 - 7.14 ft-lb/in²
Average value: 0.700 J/cm² Grade Count:16
0.0600 - 0.750 J/cm²

@Temperature -30.0 - -20.0 °C
0.286 - 3.57 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.489 J/cm² Grade Count:8
Tensile Impact Strength 84.1 - 420 kJ/m²
40.0 - 200 ft-lb/in²
Average value: 330 kJ/m² Grade Count:16
Dart Drop, Total Energy 8.00 - 14.0 J
5.90 - 10.3 ft-lb
Average value: 10.9 J Grade Count:7
Coefficient of Friction 0.170 - 0.600
0.170 - 0.600
Average value: 0.364 Grade Count:15
Coefficient of Friction, Static 0.100 - 0.620
0.100 - 0.620
Average value: 0.313 Grade Count:8
Tensile Creep Modulus, 1000 hours 2500 - 8300 MPa
363000 - 1.20e+6 psi
Average value: 4360 MPa Grade Count:5
K (wear) Factor 4.50 - 266 x 10-8 mm³/N-M
2.23 - 132 x 10-10 in³-min/ft-lb-hr
Average value: 75.5 x 10<sup>-8</sup> mm³/N-M Grade Count:8
Electrical Properties Metric English Comments
Electrical Resistivity 1.90 - 3.00e+17 ohm-cm
1.90 - 3.00e+17 ohm-cm
Average value: 1.46e+16 ohm-cm Grade Count:94
Surface Resistance 10.0 - 3.00e+16 ohm
10.0 - 3.00e+16 ohm
Average value: 9.09e+14 ohm Grade Count:40
Insulation Resistance 1000 - 1.00e+14 ohm
1000 - 1.00e+14 ohm
Average value: 2.55e+13 ohm Grade Count:4
Static Decay 2.00 sec
2.00 sec
Average value: 2.00 sec Grade Count:4
Dielectric Constant 2.80 - 3.75
2.80 - 3.75
Average value: 3.19 Grade Count:48
Dielectric Strength 12.4 - 130 kV/mm
315 - 3300 kV/in
Average value: 23.5 kV/mm Grade Count:58
Dissipation Factor 0.000700 - 0.0200
0.000700 - 0.0200
Average value: 0.00378 Grade Count:46