Physical Properties Metric English Comments
ESCR 100% Igepal® 60 hour
60 hour
Condition A; ASTM D1693
A. Schulman LP477-01 High-Density Polyethylene
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph..
ESCR 100% Igepal® 60 hour
60 hour
Condition A; ASTM D1693
A. Schulman LP477-01 High-Density Polyethylene
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph..
ESCR 100% Igepal® 60 hour
60 hour
Condition A; ASTM D1693
A. Schulman LP477-01 High-Density Polyethylene
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph..
ESCR 100% Igepal® 60 hour
60 hour
Condition A; ASTM D1693
A. Schulman LP477-01 High-Density Polyethylene
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph..
ESCR 100% Igepal® 60 hour
60 hour
Condition A; ASTM D1693
A. Schulman LP477-01 High-Density Polyethylene
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph..
ESCR 100% Igepal® 60 hour
60 hour
Condition A; ASTM D1693
Chevron Phillips Marlex® K605 HDPE Blow Molding Resin
Resin Type: Ethylene HomopolymerCharacteristics: Good ESCRExceptional rigidityExcellent melt strengthApplications: Automotive bumper beamsInformation provided by Chevron Phillips.
ESCR 100% Igepal® 60 hour
60 hour
Condition A; ASTM D1693
Chevron Phillips Marlex® K608 HDPE Extrusion Molding Resin
Resin Type: Ethylene HomopolymerCharacteristics: Good ESCRExceptional RigidityExcellent melt strengthGood whiteness in unpigmented partsApplications: Table topsNursery containersDunnage traysLarge t..
ESCR 100% Igepal® 60 hour

@Temperature 50.0 °C
60 hour

@Temperature 122 °F
F<sub>50</sub>; Molded and tested in accordance with ASTM D4976; ASTM D1693
Dow UNIVAL™ DMDA-6220 NT 7 High Density Polyethylene Resin (HDPE)
Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6220 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol..
ESCR 100% Igepal® 60 hour
60 hour
Condition B, F50; ASTM D1693
Amco PRIMATOP HDPE 004955HP Blow Molding Polyethylene
HDPE 003955PZ features zinc stearate additive and is used for injection blow molding.Former A-Top Polymers product; part of Amco product line since 2013.
ESCR 100% Igepal® 60 hour
60 hour
Condition A; ASTM D1693
A. Schulman LP477-01 High-Density Polyethylene
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph..