A. Schulman LP477-01 High-Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman LP477-01 High-Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and pharmaceutical packages. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.955 g/cc
0.955 g/cc
ASTM D792
ESCR 100% Igepal® 60 hour
60 hour
Condition A; ASTM D1693
Melt Index of Compound 0.30 g/10 min
0.30 g/10 min
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.1 MPa
3200 psi
2"/min; ASTM D638
Elongation at Break 400 %
400 %
2"/min; ASTM D638
Flexural Modulus 0.827 GPa
120 ksi
ASTM D882