Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | 300 hour | 300 hour | |
Polimeros Mexicanos Rotolene® 93050 Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene for rotational molding. This resin is fully UV8 stabilized.Recommended for general purpose applications. Frequently used for water tanks (less tha.. |
|||
ESCR 10% Igepal® | 300 hour | 300 hour | |
Polimeros Mexicanos Rotolene® Diesel Tank Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene. This resin is fully UV8 stabilized.High quality Polyethylene compound specially designed for automotive applications, water tanks, diesel tanks a.. |
|||
ESCR 10% Igepal® | >= 300 hour | >= 300 hour | ARM Method |
Borealis Borecene™ RM8342 Linear Polyethylene for Rotational Molding Borecene RM8342 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro.. |
|||
ESCR 10% Igepal® | >= 300 hour | >= 300 hour | ARM Method |
Borealis Borecene™ RM8342RC Linear Polyethylene for Rotational Molding Borecene RM8342RC is a third generation linear medium density natural polyethylene for rotational molding. Borecene RM8342RC is a special grade, which has passed many rigorous tests and can be cons.. |
|||
ESCR 10% Igepal® | >= 300 hour | >= 300 hour | ARM Method |
Borealis Borecene™ RM8343 Linear Polyethylene for Rotational Molding Borecene RM8343 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro.. |
|||
ESCR 10% Igepal® | >= 300 hour | >= 300 hour | ARM Method |
Borealis Borecene™ RM8343RC Linear Polyethylene for Rotational Molding Borecene RM8343RC is a third generation linear medium density natural polyethylene for rotational molding. Borecene RM8343RC is a special grade, which has passed many rigorous tests and can be cons.. |
|||
ESCR 10% Igepal® | >= 300 hour | >= 300 hour | ASTM D1693, Cond. B |
Total HDPE B5845 High Density Polyethylene - Blow Molding Resin Bimodal HDPE Blow Molding ResinCharacteristics:Excellent stress cracking resistanceExcellent stiffnessApplications:Household chemicalsIndustrial chemicalsIndustrial partsFood packagingPersonal care .. |