Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis Borecene™ RM8343RC Linear Polyethylene for Rotational Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Rotational Molded
Manufacturer Borealis
Trade Name Borecene™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borecene™ RM8343RC Linear Polyethylene for Rotational Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borecene RM8343RC is a third generation linear medium density natural polyethylene for rotational molding. Borecene RM8343RC is a special grade, which has passed many rigorous tests and can be considered as a possible replacement for crosslinkable polyethylene in many applications. The narrow molecular weight distribution imparted through metallocene catalyst technology provides an ideal balance of flow and physical properties. Borecene RM8343RC is delivered as powder.Borecene RM8343RC can be considered as a possible replacement for crosslinkable products in rotational molding such as fuel tanks and tanks.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.934 g/cc
0.0337 lb/in³
ASTM D1505
ESCR 10% Igepal® >= 300 hour
>= 300 hour
ARM Method
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.9 MPa
2600 psi
At 50 mm/min; ASTM D683 IV
Flexural Modulus 0.490 GPa
71.0 ksi
At 2 mm/min; ASTM D790
Dart Drop Total Energy 210.0 J/cm
0.3934 ft-lb/mil
(-4oF/-20°C); ASTM D3763
Dart Drop 152 g/micron
3860 g/mil
Instrumented Falling Weight (-4°F/-20°C); ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 65.0 °C
149 °F
ASTM D648
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Users viewing this material also viewed the following: