Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | 40 hour | 40 hour | F<sub>50</sub>; ASTM D1693 |
Petromont 3000 High Density Polyethylene Resin Petromont HDPE 3000 is a high density polyethylene resin produced using the UNIPOL® Process. This resin is designed for injection moulding applications such as crates, cases, trays, tote bins and o.. |
|||
ESCR 10% Igepal® | >= 40 hour | >= 40 hour | ASTM D1693 |
Borealis Borstar® MB7541 High Density Polyethylene for Injection Molding Borstar MB7541 is a bimodal, natural, high density polyethylene produced by the Borstar PE technology. Borstar MB7541 combines excellent organoleptic properties, Environmental Stress Crack Resistan.. |
|||
ESCR 10% Igepal® | >= 40 hour | >= 40 hour | ASTM D1693 |
Borealis Borstar® MB7542 High Density Polyethylene for Injection Molding Borstar MB7541 is a bimodal, natural, high density polyethylene produced by the Borstar PE technology. Borstar MB7541 combines excellent organoleptic properties, Environmental Stress Crack Resistan.. |
|||
ESCR 10% Igepal® | 40 hour @Temperature 50.0 °C |
40 hour @Temperature 122 °F |
ASTM D1693B |
ExxonMobil LLDPE L L6101RQ Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6101 series are medium flow LLDPE grades, which offer excellent stiffness, heat distortion resistance and good environmental stress crack resistance. The excellent toughness .. |
|||
ESCR 10% Igepal® | 40 hour @Temperature 50.0 °C |
40 hour @Temperature 122 °F |
ASTM D1693B |
ExxonMobil LLDPE LL 6101XR Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6101 series are medium flow LLDPE grades, which offer excellent stiffness, heat distortion resistance and good environmental stress crack resistance. The excellent toughness .. |
|||
ESCR 10% Igepal® | >= 40 hour | >= 40 hour | ASTM D1693 |
Borealis Bormed™ HE7541-PH HDPE for Healthcare Applications Bormed HE7541-PH is a bimodal, natural, high-density polyethylene produced by the Borstar PE technology. Bormed HE7541-PH combines low volatiles with high Environmental Stress Crack Resistance (ESC.. |