Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil LLDPE LL 6101XR Linear Low Density Polyethylene Resin (European Grade)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Exxon Chemical
Trade Name LLDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LLDPE LL 6101XR Linear Low Density Polyethylene Resin (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LL 6101 series are medium flow LLDPE grades, which offer excellent stiffness, heat distortion resistance and good environmental stress crack resistance. The excellent toughness and ESCR make LL 6101 grades an excellent blend partner for HDPE, where it can enhance the ESCR of items like buckets and lids. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal Stabilizer: Yes Applications: Bottle CapsCompounding (RQ version)ContainersDoor MatsDust BinsLarge Part HousewaresLidsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ExxonMobil method
ESCR 10% Igepal® 40 hour

@Temperature 50.0 °C
40 hour

@Temperature 122 °F
ASTM D1693B
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 10.3 MPa
1500 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Elongation at Yield 20 %
20 %
ASTM D638
Flexural Modulus, 1% Secant 262 MPa
38000 psi
ASTM D790
Izod Impact, Notched (ISO) 46.2 kJ/m²
22.0 ft-lb/in²
ISO 180/1A
Thermal Properties Metric English Comments
Melting Point <= 253 °C
<= 487 °F
Peak Melting Point; ExxonMobil method