Physical Properties Metric English Comments
ESCR 10% Igepal® >= 75 hour

@Temperature 50.0 °C
>= 75 hour

@Temperature 122 °F
F<sub>0-</sub>; ASTM D1693
NOVA Chemicals Novapol® HP-Y353-A HDPE Pipe Coating Resin
Good ESCR, Excellent toughness, High strength, Excellent processability, Excellent stiffnessApplications: For profile, corrugated non-pressure pipes, For storm and sanitary sewer pipe, For culvert a..