Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.0551 cc-mm/m²-24hr-atm | 0.140 cc-mil/100 in²-24hr-atm | 37°C; 90% RH |
Parylene Coating Services C Poly (P-Xylylene) Monomer is monochloro para-xylylene. Parylene C is recommended where excellent barrier protection is needed. It can be used up to 125°C where oxygen is present.Parylene is a generic name for poly-.. |