Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.100 cc-mm/m²-24hr-atm | 0.254 cc-mil/100 in²-24hr-atm | ASTM F1249 |
Chevron Phillips HiD® 9662 HDPE Blown Film Resin
(discontinued **) Resin Type: Linear Polyethylene HomopolymerCharacteristics: Unique Molecular Architecture Gives Outstanding Moisture Barrier Properties, Excellent Film Strength and Toughness for a Homopolymer, Give.. |
|||
Moisture Vapor Transmission | 0.100 cc-mm/m²-24hr-atm | 0.254 cc-mil/100 in²-24hr-atm | ASTM F1249 |
Chevron Phillips MarFlex® 9659 HDPE Blown Film Resin Resin Type: Linear Polyethylene HomopolymerCharacteristics: Unique Molecular Architecture Gives Outstanding Moisture Barrier Properties, Excellent Film Strength and Toughness for a Homopolymer, Give.. |
|||
Moisture Vapor Transmission | 0.100 cc-mm/m²-24hr-atm | 0.254 cc-mil/100 in²-24hr-atm | ASTM E96 Procedure E |
DuPont Teijin Films Mylar® M33 Polyester Film, 50 Gauge, PVDC Coated Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. the coating is heat sealable, and is an excellent moisture and.. |