Polymer Property : Moisture Vapor Transmission = 0.570 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.570 cc-mm/m²-24hr-atm
1.45 cc-mil/100 in²-24hr-atm
g.mm/m2.day; 37.8°C (100°F) and 90% relative humidity (ASTM F 1249)
Advanced Elastomer Systems Trefsin® 3201-65 W305 Thermoplastic Rubber  (discontinued **)
A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t..
Moisture Vapor Transmission 0.570 cc-mm/m²-24hr-atm
1.45 cc-mil/100 in²-24hr-atm
ASTM 1249
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack..
Moisture Vapor Transmission 0.570 cc-mm/m²-24hr-atm
1.45 cc-mil/100 in²-24hr-atm
Proc. E; ASTM E96
DuPont Teijin Films Mylar® OL12 Polyester Packaging Film, 150 Gauge
Data provided by DuPont Packaging Polymers.Mylar® OL12 (formerly known as XM963A) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sea..
Moisture Vapor Transmission 0.570 cc-mm/m²-24hr-atm
1.45 cc-mil/100 in²-24hr-atm
g.mm/m2.day; 37.8°C (100°F) and 90% relative humidity (ASTM F 1249)
Advanced Elastomer Systems Trefsin® 3101-65 W305 Thermoplastic Rubber  (discontinued **)
A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec..