Physical Properties Metric English Comments
Moisture Vapor Transmission 0.630 cc-mm/m²-24hr-atm
1.60 cc-mil/100 in²-24hr-atm
ASTM 1249
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 100 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab..
Moisture Vapor Transmission 0.630 cc-mm/m²-24hr-atm
1.60 cc-mil/100 in²-24hr-atm
ASTM 1249
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 100 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of ..
Moisture Vapor Transmission 0.630 cc-mm/m²-24hr-atm
1.60 cc-mil/100 in²-24hr-atm
g-mm/m²-day; based on 1 mil (0.0254 mm) thick film; ASTM E96
DuPont Elvax® 3128 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film  (discontinued **)
8.9 wt% Vinyl Acetate.Elvax® 3128 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resin..
Moisture Vapor Transmission 0.630 cc-mm/m²-24hr-atm
1.60 cc-mil/100 in²-24hr-atm
ASTM 1249
DuPont™ Clysar® EZ Polyolefin Shrink Packaging Film, 50 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film. Clysar® EZS is a high slip version of EZ. Used where a premium product appearance ..