Polymer Property : Moisture Vapor Transmission = 1.12 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.440 cc-mm/m²-24hr-atm
1.12 cc-mil/100 in²-24hr-atm
ASTM 1249
DuPont™ Clysar® VHP Polyolefin Shrink Packaging Film, 50 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.DuPont Clysar® VHP is a thin gauge, clear, biaxially oriented, heat shrinkable polyolefin film. It provides strong seals and excellent optics under a wide..